If I get time on Monday, I'll answer more fully (trying to get the
weekend started just now in the UK!), but there is an alternative
solder on the market called Colophony free solder which is rosin free
but I'm I'm still not decided on it yet.
Best Regards
Ian Boyton
>From: Ryan Chase <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>,Ryan Chase
<[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Corrosion
>Date: Wed, 14 Apr 1999 17:25:29 MDT
>MIME-Version: 1.0
>From [log in to unmask] Wed Apr 14 16:34:14 1999
>Received: from [208.150.51.11] by hotmail.com (1.5) with SMTP id
MHotMailB8DE70CA018ED1B98316D096330B12E81; Wed Apr 14 16:34:14 1999
>Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for
Windows NT v1.1a) with SMTP id <[log in to unmask]>; Wed, 14
Apr 1999 18:24:09 -0500
>Received: from JEFRY.IPC.ORG by JEFRY.IPC.ORG (LISTSERV-TCP/IP
release 1.8c)with spool id 1871789 for [log in to unmask]; Wed, 14
Apr 199918:24:08 -0500
>Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for
Windows NTv1.1a) with SMTP id <[log in to unmask]>; Wed, 14 Apr
199918:24:08 -0500
>Approved-By: [log in to unmask]
>Received: from simon.ipc.org by jefry.ipc.org (LSMTP for Windows NT
v1.1a) withSMTP id <[log in to unmask]>; Wed, 14 Apr 1999
18:19:10 -0500
>Received: from outmail.hdap.com by simon.ipc.org via ESMTP
(951211.SGI.8.6.12.PATCH1502/940406.SGI) for <[log in to unmask]>
idSAA27317; Wed, 14 Apr 1999 18:08:18 -0700
>Received: from chaps.hdap.com ([192.168.10.5]) by outmail.hdap.com
(Post.OfficeMTA v3.5.1 release 219 ID# 0-0U10L2S100V35) with ESMTP id
com for<[log in to unmask]>; Wed, 14 Apr 1999 17:30:10 -0600
>Received: from CHAPS/SpoolDir by chaps.hdap.com (Mercury 1.43); 14
Apr 9917:25:42 MST -0700
>Received: from SpoolDir by CHAPS (Mercury 1.43); 14 Apr 99 17:25:35
MST -0700
>Priority: normal
>X-mailer: Pegasus Mail for Win32 (v3.01d)
>Message-ID: <[log in to unmask]>
>Sender: TechNet <[log in to unmask]>
>Organization: GE HARRIS Energy Control Systems
>
>Has anyone heard of rosin based fluxes causing corrosion?
>
>It is on a connector with solder cup connections and the flux used is
>a RA flux. The pins and the solder is showing signs of corrosion.
>Could this be caused or accelerated by the flux?
>
>Any help is appreciated.
>
>Ryan
>
>-----------------------
>Ryan Chase
>Manufacturing Engineer
>GE Harris
>403-214-4502
>Fax 403-287-3107
>[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|