Bob,
My two cents for the Friday - If I read the question correctly, you are
asking about adhering either a 0.1um tin plated part, or a 2um tin plated
part to bare, non-metallized FR-4.
Given that the tin plated components are virgin/not oxidized, it is my
belief that the adhesive will adhere much better to the bare FR-4 than to
either of the tin plated components. In the virgin state, I would not
expect much, if any difference between them.
Should the Sn plated components have been subjected to a thermal exposure of
some kind - what was formerly beneath the thin Sn plating may now also be
oxidized and corrupting the surface making it's interface weaker sooner.
Heat cure adhesive, UV, or room temp? - I am not a great fan of adhesively
bonding [long term] to Sn. The higher the heat cure, likely the worse it
will get.
Will see how much other traffic this starts :-)
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of bob wettermann
Sent: Thursday, April 09, 2009 11:17 AM
To: [log in to unmask]
Subject: [TN] Friday Theorizing
Dear Technetters:
Has anyone done any adhesion testing of a 2um tin-electrocoated surface
(copper carrier) to FR-4? How about a 0.100um tin electrocoated surface? Can
someone theorize on which might give better adhesion using a 2-part epoxy?
Regards
Bob Wettermann
BEST
PH 847-767-5745
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|