Ingemar - Joyce,
My limited experience with the eximer for ablation was that even though the
laser removed the organics, I still [understandably] had to deal with the
inorganics left behind - such as silica with a PEMs device.
Whether I blew it off, or washed/rinsed it off, it broke up a potentially
nice process a great deal. This was back in the olden days. To some
extent, each pulse would dislodge some of the filler ... but not enough.
Possibly provisions have been made for this by now.
Still, it is better than smelly-messy Decap, or the hazards of fuming
nitric...
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|