As long as the PCB samples represents all design variations in the board and provide the correct number of hole locations you are OK. So, for example, internal annular ring you need all layers represented in a 3 hole pattern, both in x and y diagonal corners. In this case if the board location is not serialized, you are not able to adequately complete this test as the PCB could be side by side on the panel, or even rotated x/y negating the 2 axis validation. There are several test considerations that have similar issues. One piece of trivia is we have found getting all testing requirements done on a PCB will generally give you a more accurate view into the reliability.
Jeffrey Bush
BAE Systems Incorporated
IS&R - Space Products and Systems
P.O. Box 868, MER24-116A
Nashua, NH 03061-0868
Office +1 603.885.8137
Mobile +1 603.318.8056
Fax +1 603.885.5258
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro
Sent: Monday, June 20, 2011 1:12 PM
To: [log in to unmask]
Subject: [TN] Using PWBs instead of test coupons to meet IPC-6012 Class 3
I recently came across a situation where PWBs were used in lieu of test
coupons to meet a contractual 3rd party micro-section test requirement
for IPC-6012 Class 3 hardware.
This decision was made after having the PWBs stored in the stockroom for
two years.
I was asked to get involved when the PWB "coupon" failed for
Solderability testing by the 3rd party test house.
I checked and the original PWB micro-section report from the fabricator
indicated that the test coupons all passed at the time of manufacture.
So I am left wondering about the requirement that is intended by 6012 to
use test coupons.
I would have thought at the very least, the PTH hole locations of PWB
which would correspond to the test coupon sections would have to have
been identified and approved.
I can rationalize why the stored board would not meet Solderability
requirements after two years in a stockroom, but I cannot get past the
requirement to use actual test coupons for acceptance testing.
Am I missing something or do we have a choice whether to test the
coupons vs the actual PWB?
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|