There are composite pwb materials with matched CTE's to silicon etc and therefore to Kovar/42
alloy etc, but these tend to be expensive.
I am a little puzzled on this, maybe I am out of touch, but can you explain why the CTE of the
leads is important to you?
Alloy 42 has been a standard lead frame material for years. So far as I understand it the usual
reason for device manufacturers changing to copper is to improve thermal conductivity from their
device, which is worth the extra difficulties involved.
Mike
----- Original Message -----
From: Louis, Edwin @ CSE <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, February 18, 2000 7:10 PM
Subject: [TN] Alloy 42 Leaded TSOPS
> We have a sole source for TSOP components, in which, they are only
> available with alloy 42 leads. The vendor refuses to build the parts with
> Copper leads because the CTE of alloy 42 better matches the die CTE and as
> result they have fewer component failures and defects.
>
> Does any one know of a PWB material that would better match the CTE of alloy
> 42 leaded TSOPs?
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|