TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=ISO-8859-1
X-To:
Date:
Fri, 28 Apr 2006 14:22:55 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (38 lines)
If you HAVE TO use parts like that, try a low CTE PCB material, such as Arlon 85NT.  This is nice stuff, with a listed CTE under 10ppm/C.  It goes up a bit with high copper loading.  Very stable, Tg over 200C, but sucks up moisture and is hell to board route without the edge fuzzing due to the aramid fibers.

>>> [log in to unmask] 4/28/2006 1:47:58 pm >>>
Hi Ioan,
Castellated ceramic leadless chip carriers were a bad idea when the were 
developed in the '80s, and nothing has changed*oops, I forgot about that SAC-stuff 
making things worse.
The problem is not the 'castellations' per se, but the fact that they will 
not allow the CC to swim up. Thus, the solder joint thickness is at a minimum, 
producing the worst-possible SJ reliability geometry--if you shim up the CC to 
increase SJ height, you can get about the same as what you get with BGAs with 
the same ball dimension.
Putting large ceramic components on FR-4, castellated or not, is not a good 
idea.


Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2