TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 22 Mar 2006 14:11:27 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, arnaud grivon <[log in to unmask]>
Subject:
From:
arnaud grivon <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (148 lines)
Amol,

Could you expand on the kind of defects you experienced (cross section 
pictures) and clarify your "testing was a hassle" statements?

Phil Nutting a écrit :
> Thanks Amol.  I'll look at this more closely. 
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
> Sent: Wednesday, March 22, 2006 7:17 AM
> To: [log in to unmask]
> Subject: Re: [TN] mixing lead-free solders
>
> Hi Phil,
> Based on the info in the e-mail, you say you are using SAC305 in the
> wave.......did you do any testing that proved that SAC305 was superior
> than SN alloy in wave? Or is this an absolute requirement for the
> product/process?
>
> We used SAC 305 in wave and ended up with Hot Tears on greater than 90%
> of all TH joints........you may have the following issues
>
> 1. if you get hot tears, current IPC spec is not sufficient to pass/fail
> them (because it is impossible to see the bottom of any of the tears @
> magnifications mentioned in IPC 610)
> 2. I did some X-sectioning and X-ray analysis of our samples, and even
> though they turned out OK as per IPC, testing them was a hassle to say
> the least.
>
> So be careful before using SAC305 in wave.
>
> Good Luck
>
> Amol Kane
> M.S (Industrial Eng.)
> Process Engineer
> Harvard Custom Manufacturing 
> 941 Route 38  Owego, NY 13827
> Phone: (607) 687-7669 x349
> [log in to unmask]
>
>  -----Original Message-----
> From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Whittaker, Dewey
> (AZ75)
> Sent:   Tuesday, March 21, 2006 4:36 PM
> To:     [log in to unmask]
> Subject:        Re: [TN] mixing lead-free solders
>
> I've seen several presentations that shows that to be an effective
> combination. All other things being equal, you should be fine.
> Dewey 
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
> Sent: Tuesday, March 21, 2006 2:07 PM
> To: [log in to unmask]
> Subject: [TN] mixing lead-free solders
>
> Good afternoon,
>  
> As we move further into LF conversion I was curious what you, the gurus
> of TechNet, thought about the possibility of mixing LF solder alloys.
>  
> We are converting our manufacturing operation to SAC 305 for wave and
> hand solder.  We have a CM that is using Sn100C in their wave.  There is
> the potential to have to manually repair a board built with Sn100C by
> hand soldering with SAC 305.  Are there any reliability issues with
> this?  Assume the board will be properly cleaned after soldering.
>  
> I haven't looked into our SMT CM and their process, but it could be
> similar.
>  
> I'd hate to have to run three or four lines to keep each alloy separate.
> As it is I must manage Sn/Pb and SAC 305.
>  
> Thanks in advance.
>  
> Phil
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>   

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2