I have a conveyorized system from which a board passes from a alkaline
cleaner running at 50 C to a cold water rinse. The differential in
temperature, along with the alkalinity is causing calcium build up in my
rinse.
Do you think this type of unit will stop this or do I need to remove the
calcium through typical soft water treatment.
Ted
----------
From: Mark Austin <[log in to unmask]>
To: [log in to unmask]
Subject: Re: [TN] Removing calcium from water
Date: Wednesday, June 16, 1999 7:52 AM
Yes, I've used one.
The cost is about £30 sterling.
They are maintenance free.
They are claimed to last forever, as long as the magnetic field is present.
They are not as good as a traditional water softener. I have found that
they
don't totally soften the water (they don't remove any chemicals). They work
(I seem to remember) by aligning all the ions in the water the same way
which some how stops the hard water chemicals from sticking to anything.
If you need to remove the hard water chemicals use a traditional water
softener (Resin type)
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
15/06/99 20:10
>Has anybody heard of, or used a device that is basically a magnetic type
>filter (so I'm told) that is used in line to soften water.
>
>If so I would appreciate any info:
> - approx cost compared to typical water softner
> - maintenance
> - life expectancy
> - efficiency
>
>Ted
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
Mark Austin (Process Engineer)
ACW Technology Limited
Hylton Road
Petersfield
GU32 3XX
ENGLAND
TEL - +44 (0) 1730 300000
FAX - +44 (0) 1730 266045
Email - [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
----------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|