Subject:
From:
Tenison Stone <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 12 Dec 2003 10:39:02 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (114 lines)
Steve,

As usual you are the expert.  How do you remember where to find all this
stuff?

I need to update your link for the cookson white paper:

http://www.speedlinetech.com/DOCS/White_Papers/EquipmentImpactsofLeadFreeWavesolderingAPEX2003BestUSPaper.pdf

I am planning on replacing the current machine.  It would take too many
modifications for lead free.

Tenison Stone
Manufacturing Engineer
Telex Communications
1930 West First Street
Blue Earth, MN  56013
507-526-3205   x2164
507-526-3059 (fax)




Steve Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/12/2003 10:14 AM
Please respond to "TechNet E-Mail Forum."; Please respond to SteveZeva


        To:     [log in to unmask]
        cc:
        Subject:        Re: [TN] wave solder specifications for lead free


Hi Tenison!

You have more than just the pot to worry about, pumps, nozzels, ducting
are
things that can get eaten-up as well.

At this past APEX, there was a good paper published called; "Equipment
Impacts of Lead Free Wave Soldering" that can be a good reference. It's
at:

http://www.cooksonee.com/DOCS/White_Papers/EquipmentImpactsofLeadFreeWavesolde
ringAPEX2003BestUSPaper.pdf

And another good resource is at:

http://www.alphametals.com/products/lead_free/tech_art.html

Hope this helps,

-Steve Gregory-





> Good morning,
>
> I have been given the task of finding out what is needed in a wave
solder
> machine to go lead free.   We have an old Hollis machine that will not
> handle the new lead free temperatures, so I know I need longer preheat
> sections.  I also need a new pot since it is the original design and
will
> not withstand lead free solder compositions proposed.  I will also
specify
> a nitrogen blanket.
>
> Please divide your list among needed and frills that might be fun, but
are
> not absolutely necessary.  I want to make sure I am not missing anything
> in my specifications.
>
> Thank you in advance.
>
> Tenison Stone
> Manufacturing Engineer
> Telex Communications
> 1930 West First Street
> Blue Earth, MN  56013
> 507-526-3205   x2164
> 507-526-3059 (fax)
>


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2