TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Tan Geok Ang <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Tan Geok Ang <[log in to unmask]>
Date:
Thu, 15 Jan 2009 09:26:40 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (46 lines)
Hi Steve,

            Please help to download these pictures TechNet, thanks.

     

 

 

Hi All experts,

            Testing (combine test of 16G at 85 oC) was performed on
evaluation boards with under-filled BGAs. Open issue (cracks) was
detected only at some corners of the BGA (35x35mm with 1156 balls) after
the test. Lead-free process and PCB with ENIG surface finish. Peak
temperature is 248 oC with a 65 sec above 217 oC. 

FYI, the service lab has not come out a report.

            What are the possible causes? (CET mismatches, Lead-free
alloy related, material, processes)

 

            Thank you in advance.

 

Regards

GA Tan

  


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2