Hi Steve,
Please help to download these pictures TechNet, thanks.
Hi All experts,
Testing (combine test of 16G at 85 oC) was performed on
evaluation boards with under-filled BGAs. Open issue (cracks) was
detected only at some corners of the BGA (35x35mm with 1156 balls) after
the test. Lead-free process and PCB with ENIG surface finish. Peak
temperature is 248 oC with a 65 sec above 217 oC.
FYI, the service lab has not come out a report.
What are the possible causes? (CET mismatches, Lead-free
alloy related, material, processes)
Thank you in advance.
Regards
GA Tan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|