Bev,
What type of Pd? Plated, evaporated, Pd/Ag? The dissolution rate is Pd
process dependent (not all Pd are made equal).
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>Dave Hillman
>Sent: Thursday, July 31, 2003 3:51 PM
>To: [log in to unmask]
>Subject: Re: [TN] Thick Palladium on Leads
>
>
>Hi Bev! You need to be careful with the Pd thickness. When
>soldering to thick Pd plating layers you can potentially have
>problems with "Pd embrittlement" of the solder joint. Pd and
>Sn for an intermetallic phase
>(PdSn4) which behaves in the same fashion as the AuSn4
>intermetallic phase for gold embrittlement of solder joints.
>There are two industry reference I know of off the top of my
>head - the NCMS Surface Finishes Study and a Collins paper
>published at the 1996 SMI conference. If you keep the Pd
>thickness between 9-15 microinches you should be able avoid
>the PdSn4 phase with a controlled soldering processes. Also
>note that Pd has a very slow diffusion rate so you may have to
>adjust your soldering process times. Good Luck.
>
>Dave Hillman
>Rockwell Collins
>[log in to unmask]
>
>
>
> Bev Christian
> <[log in to unmask] To:
>[log in to unmask]
> ET> cc:
> Sent by: TechNet Subject: [TN]
>Thick Palladium on Leads
> <TechNet@listserv
> .ipc.org>
>
>
> 07/31/2003 12:28
> PM
> Please respond to
> "TechNet E-Mail
> Forum."; Please
> respond to Bev
> Christian
>
>
>
>
>
>
>Technetters,
>I have searched the archives and all I have been able to find
>is one informative e-mail from Phil Hinton from August 22,
>1998. Has anyone every run across palladium as a thick
>undercoat? if so, what, if any, grief did it cost you?
>
>regards,
>Bev Christian
>Research in Motion
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|