TECHNET Archives

April 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 6 Apr 2018 15:10:08 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Muller, Mary" <[log in to unmask]>
Message-ID:
Subject:
From:
"Muller, Mary" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (30 lines)
This section of IPC-A-610 correctly defines any fracture of any solder joint as a defect for all 3 classes.

Mary Muller
IPC-A-610 Co-Chair
Sr. Supplier Quality Engineer
Crane Aerospace and Electronics

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, April 05, 2018 7:48 AM
To: [log in to unmask]
Subject: [TN] IPC-A-610G, section 5.2.9,, Solder anomalies-Fractured solder, Defect 1, 2, 3 (Axial leaded device)

Fellow TechNetters:

   Is there a percentage associated with the statement "Fractures Solder" in the above stated IPC STD section?
I did not a similar statement, Fractured Solder, for Surface Mount Devices and Surface Mount Area.
Is there an acceptable percentage of the solder joint lead interface that can be fractured?


Victor,


________________________________
Connect with us on LinkedIn<http://www.linkedin.com/companies/crane-aerospace-electronics>!
We value your opinion! Please click the survey link to tell us how satisfied you are: http://www.craneae.com/VOC
Crane Aerospace & Electronics Confidentiality Statement:
The information contained in this email message may be privileged and is confidential information intended only for the use of the recipient, or any employee or agent responsible to deliver it to the intended recipient. Any unauthorized use, distribution or copying of this information is strictly prohibited and may be unlawful. If you have received this communication in error, please notify the sender immediately and destroy the original message and all attachments from your electronic files.
________________________________

ATOM RSS1 RSS2