We currently use an electrowinning unit to remove most of the gold
from the drag-out rinse following gold plating. The unit consists of
a cylindrical inert anode surrounding a copper metallized plastic
cathode. We remove the cathode when it has about 60 oz. of gold
plated on it. You can send the cathode to a gold reclamation/refining
company. We have a high temp furnace on site so we can melt down the
cathode to ingots which give about 10% higher return from the refiner.
After the electrowinner, we use ion exchange to remove the remaining
gold to below 1ppm. The IX system consists of three 1-cubic foot
columns. We have to replace one of the columns about every six months
when it beomes spent with gold and cyanide. We send the resin off
site for reclamation.
We use Engelhard in the Anaheim, CA for our reclamation/refining of
gold, but there are many others out there to choose from.
Contact me off-line if you would like specific information on the
electrowinning or other equipment.
Michael Holan
Process Engineer
HADCO-Austin
512-246-5612
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: [TN] Gold drag out reclaim
Author: Albert Mok <[log in to unmask]> at smtplink-hadco
Date: 4/8/99 11:29 PM
As everyone may try to recover the solution of gold drag out bath which is
immediately followed by gold plating bath.
I am thinking about options like electrowinning, carbon absorption or even
concentrated it and put the solution back to the gold bath. Do you have
this experience and I desperately look for your input.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|