TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 14 Nov 2008 12:14:21 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Frank Kimmey <[log in to unmask]>
Subject:
From:
Frank Kimmey <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (117 lines)
Victor,
We also use a lot of these filter caps.
I am not sure about the IPC but I do think the end terminations are to small.
It looks like ~50% of the end termination is solderable, so you may have some issues like reliability and definitely self centering (as your photos show).
I would definitely recommend a larger pad, equal to or slightly larger (~10%) than the end termination of the part.
You might be Ok with as designed but I would not want to bet on it without reliabilties but in.
Werner or some others could probably tell you if the solder joint is enough to have the warm and fuzzy.
Sorry not to have more,
FNK

Frank N Kimmey CID+
Manager - PCB Design
Global Product Development
Powerwave Technologies Inc
Mobile 916-670-0645

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, November 14, 2008 11:51 AM
To: [log in to unmask]
Subject: Re: [TN] Strange looking ceramic component

Steve,

   Thanks for posted my photos.   I hope to get some interesting
comments.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, November 14, 2008 1:37 PM
To: [log in to unmask]
Subject: Re: [TN] Strange looking ceramic component

Hi Victor,

Sorry for not getting your pictures posted sooner. I've been busy with a
fire here...

Anyways, got your pics up now:

http://stevezeva.homestead.com/files/PWB-FL1-1.JPG

http://stevezeva.homestead.com/files/PWB-FL1-1a.JPG

I'm not an electrical engineer, but I do know that they are filter
capacitors used to help with EMI. We place a lot of them on quite a few
assemblies.

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, November 14, 2008 10:03 AM
To: [log in to unmask]
Subject: [TN] Strange looking ceramic component

Fellow TechNetters:

   I have a ceramic component, capacitor, with four solder joint
terminations.   My main concern is the component body size to copper pad
ratio.   Do they violate IPC standards?   I sent Steve G. some photos to
upload to his web page.

Victor,

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2