In a message dated 11/17/2003 16:52:11, [log in to unmask] writes:
>It is the preheat it the wave that is controlled (the infamous 2C/sec)
>to prevent thermal shock.
---This is correct.
>Once the chip has achieved a specified temp, all the materials have expanded
equally and >after this point the rapid thermal change of hitting the wave
does not affect the chip.
---Sorry, but there is no such condition; different materials will always
have a differentiasl thermal expansion, unless they have identical CTEs.
>It is the different expanding properties of the two materials that cause the
chip
>to crack.
---Quite correct.
>Once they have both expanded to their maximum state, the temperature curve
is irrelevant.
---Sorry again, but there is no such state; as long as you raise the
temperature materials will expand, unless they have a negaqtive CTE.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|