TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wqItX-000BlOC; Mon, 21 Jul 97 08:52 CDT
Old-Return-Path:
Date:
Mon, 21 Jul 97 09:35:17 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14137
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"DPDTw.0.zoH.vcsqp"@ipc>
Subject:
From:
>From willli Mon Jul 21 08:
53:03 1997
X-Loop:
From [log in to unmask] Mon Jul 21 16:
05:16 1997
Message-Id:
Parts/Attachments:
text/plain (39 lines)
     How can I find out more information about SERA?


______________________________ Reply Separator _________________________________
Subject: Re: Re[2]: Solder Mask Residue
Author:  [log in to unmask] at corp
Date:    7/16/97 2:56 PM


SERA is Sequential Electrochemical Reduction Analysis. The technique can 
detect and quantify the oxides and other reducible species on the metal and
 alloys surfaces. The presence of the soldermask residue can be monitored on
the copper too.
     
Regards
Mike Pavlov
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2