TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Date:
Wed, 11 Feb 2009 16:53:15 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (70 lines)
Hi Rich - we use solder/dross recovery equipment (we call them solder 
"boots" because of their shape) in three of our facilities and we put the 
recovered solder bars back into the wave solder machine. I have conducted 
a couple of metallurgical composition tests on the recovered bars to see 
if they contained an excess of any elements and did not find anything that 
I considered an issue. We have about 5-6 years of history with no issues 
to date. 

Dave



Richard Kraszewski <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
02/11/2009 12:27 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Richard Kraszewski <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Local Solder Dross Recovery & solder joint reliability






I was surprised to have searched the TechNet archives and not found much
recent discussion on this topic. 

Can I get any of your thoughts on the reliability of solder joints that
includes solder that was locally recovered from dross taken from the
same manufacturing site? 

 
Rich  Kraszewski
Plexus 

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2