IS this the same questions as we had recently?
IF the FeNiCr has been directly electroplated with a fusible (Sn Sn/Pb etc)
or a soluble (Au Ag) coating then the solder will either melt or dissolve
the coating and try to wet to the FeNiCr. And almost certainly fail. You may
achieve some low strength adhesion from mechanically keying, but essentially
expect non wetting. Components will probably fall off if you rap end of PCB
on to desk.
IF the Sn Sn/Pb etc coating has been applied by hot dipping using an
aggressive flux so that a true solder bond (intermetallic) has been formed
then should be no problems. Wetting will already have been achieved and you
will be in exact same position as with any other reflow.
I suppose the worst situation is where the components have been processed in
this way, but marginally/poorly; this will give dewetting, which may be
variable and intermittent.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Friday, October 01, 2004 9:19 PM
To: [log in to unmask]
Subject: [TN] DIP Lead Frame Base material Fe Ni Cr
Fellow TechNetters,
Can someone share their experience using an Fe Ni Cr lead frame base
metal? This base material is used without a nickel barrier alloy prior
to lead plating. What type of failures could be expected?
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|