TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Ken Patel <[log in to unmask]>
Date:
Wed, 29 Sep 1999 14:14:12 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Joan M.Slade" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Joan M.Slade" <[log in to unmask]>
Parts/Attachments:
text/plain (56 lines)
a minimum is a minimum....is a MINIMUM!!!
There for...rejectable.
----- Original Message -----
From: Ken Patel <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, September 29, 1999 1:42 PM
Subject: [TN] Hot: Copper plating thickness


> If my requirement for the copper plating is 0.001" minimum (as spelled out
> on my fab drawing) and if I am reading it between .0004"-.001", is it
> rejects or not?. I tried to look at IPC-6012 which is calling out avg
copper
> thickness. I don't how easy to get ave #. This is clearly a reject to me.
> But I am looking for an expert opinion on the subject. Via Hole in
question
> is 16 mil +3 mil / -10 mils.
>
> re,
> ken patel
> ______________________________________________________
> Ken Patel                       Phone:  (408) 490-6804
> 1708 McCarthy Blvd.             Fax:    (408) 490-6859
> Milpitas, CA 95035              Beeper: (888) 769-1808
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2