To All,
I am interested in finding out what the difference is between what is
called a laminate void, and a spot of delamination or blister.
Because of the great difference in acceptable size between the 2 defects,
it seems to be important to be able to differentiate them.
Why is such a small (anything greater than .003") void unacceptable (IPC
600 3.1.1), but a larger delamination spot acceptable as long as it doesn't
violate conditions spelled out in IPC 600 2.3.2.
Any information as to how to identify the differences, and why one is more
"acceptable" in terms of size would be greatly appreciated.
Thank you,
Brian Lane
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|