Dear Janardhan:

As most tin strippers are not diluted prior to use, a simple specific
gravity controller will suffice in most cases.  One supplier with whom I
am familiar is Walchem (508-429-1110).

Regards
Ted Stern

System Administrator wrote:
>
> Hello TechNetters,
>
>       We are looking for a Feed & Bleed System for Autodosing
> of Chemicals in our Tin Stripper. Anybody who can supply or
> give more information on whom to contact, may please reply.
>
>       We are also looking for internal spares for Quiet Drill
> 420, 820 & ABW110 spindles. Again, anybody with any information
> please reply.
>
> Thanks in Advance
> Janardhan Rao
> Email : [log in to unmask]


ATOM RSS1 RSS2