Subject: ASSY:BGA Moisture Handling 1997.12.0310:37 AM
Hi TechNetters,
I have some questions about handling of moisture sensitive BGA's (and other
components).
1. Where can I get a low RH (<5% RH) oven for baking BGA's at low temperature
(40'C) ? (Tape and Reel does not appreciate the 125'C bake for 24 hours!)
What method are you using for baking (eqmt, temp., time) ?
2. Are there other methods used to control "repeated" exposures of components
other than a "follower" which travels with the Reel / Trays ?
3. Where can I get a proper sealer for MBBs (moisture barrier bags) ? Is
there a method to verify that the seal is sufficient ?
4. Is there a commercial training package available for handling of moisture
sensitive components ?
Your help is greatly appreciated.
Charles Elliott
NPI Process Engineering
Newbridge Networks Corp.
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################