Franlin,
No tenting is not the same as plugging,it's better when done properly.
IPC has a Plugged Via Performance Task Group where much effort has been
done defining and classifying the differences.
Dewey
> -----Original Message-----
> From: Franklin D Asbell [SMTP:[log in to unmask]]
> Sent: Friday, October 24, 2003 8:05 AM
> To: [log in to unmask]
> Subject: Re: [TN] Cleaning of via holes under components
>
> Tenting or plugging? Tenting vias is not the same as plugging, with
> tenting
> the risk of entrapment is higher then with plugging, with properly
> performed
> double-side plugging (talking strictly solder mask plugging) the risk
> drops
> tremendously...to ensure absolutely no entrapment (absolute being 99.8%
> chance nothing becomes entrapped) then perhaps epoxy plugged vias...
>
> Franklin
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|