TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 8 Apr 2013 13:47:26 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (110 lines)
Many thanks Harvey.  I would very much interest to know the detail of the presentation.  The nano particles are utilized in printed electronics, in various elements and organic conductive media to improve conductivity and flexibility.  Normally, printed electronics are processed in low temperature with large surface contact area (roll to roll printing).  Therefore, it can be flexible and thin, the resistance short coming of the nano-particles due its large surface/interface characteristics (sometimes, it is hopping rather than normal conduction mechanism) are compensated by large conduction contact surfaces and thin joints.  

Sintering/fusing of the nano-particle can be done at lower temperature due to highly active surface energy, however, unless performed under pressure, you might get un-controlled re-crystallization and growth of the grain, resulted preferential growth of certain orientation of grain and leave some voids behind (low angle co-incidence grain boundary, as well as twining, are stable boundary, but not high angle gain boundary)- you might get more conductivity loss in high frequency and resistance increase. Of course, all the oxidation must be taking care of (copper is very readily oxidized, even with OSP coated, with that much surface area (nano particle).  Acid media is more less like a flux can take care some of surface oxidation, but you still need to control the coalescence and growth (not all orientation are grow at same rate...).  

The existing solder interconnect is heading towards smaller, more compact (solid) joints, for example, flip chip, or TSV for high speed, high density interconnect (in line with the high density IC with node of <20 nm).  The solder interconnect joints more in the 3D stack, rather than 2D in printed electronics.  High surface/interface might be good for some application, such as low frequency, low temperature application, I am a bit curious how it can be apply to the high frequency, high I/O, short and dense interconnect at lower voltage, and high device temperature (current processor dissipated 40-100W in some cases).  Looking forward to see the presentation (I would really appreciated if you can share with us).  I haven't been in the field for long time, Looking forward to update my knowledge.  Thanks.  My 2 cents. 
Best regards,




Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of harvey
Sent: Saturday, April 06, 2013 9:16 PM
To: [log in to unmask]
Subject: [TN] copper nanosolder--fyi

Biltmore Santa Clara for dinner (or non-dinner) 
            June 12, 2013.

Dr. Zinn's bio and abstract are at the end. 
            Lockheed's nano-copper solder is an answer to the lead-free solder 
            fiasco.
Remember "the non-solution to the non-problem",
that 
            is, until we get rid of most solder altogether, most solder paste, 
            anyhow.


            
              
              
                Speaker:
                Alfred Zinn, Lockheed Martin Space 
                  System Company ATC, Senior Scientist
              
                Abstract:
                
                  NanoCopper Materials Platform for Electronic 
                  Packaging and Printed Electronics with 200 °C Processing 
                  Temperature

                  The Advanced Technology Center of the Lockheed Martin 
                  Corporation has developed a nanocopper-based material that can 
                  be fused to bulk copper around 200 °C taking advantage of the 
                  rapidly decreasing fusion temperature with decreasing particle 
                  size at the nanoscale. The nanocopper material has the 
                  potential to replace tin-based solder to eliminate whisker 
                  growth and mechanical reliability concerns encountered with 
                  current lead-free solder. Fully optimized, the fused copper is 
                  expected to exhibit 10-15x electrical and thermal conductivity 
                  improvements over tin-based materials currently in use. The 
                  materials platform is enabled by our scalable Cu nanoparticle 
                  fabrication process employing a low cost solution-phase 
                  chemical reduction approach. A proprietary mixture of 
                  surfactants controls particle size and size distribution as 
                  well as stabilizing the particles preventing particle growth 
                  and oxidation, which would otherwise degrade its activity. We 
                  have demonstrated assembly of fully functional LED test boards 
                  using a paste formulated with nanocopper that exhibits a 
                  consistency very similar to standard tin-based solder paste. 
                  To date, we have demonstrated 26-pin through-hole connector 
                  assembly and a variety of surface mount components. We 
                  demonstrated feasibility of drop-in solder replacement using 
                  standard stencil and pick & place packaging equipment as 
                  well as demonstrated feasibility of using the material for 
                  printed electronics applications.
              
                 
                Dr. Zinn 
                  received his Doctor of Science degree in Chemistry in 1990 
                  from the Philipps University, Marburg, Germany. Following 
                  completion of his graduate studies, Dr. Zinn spent five years 
                  at UCLA as a lecturer and conducting postdoctoral research on 
                  low-temperature CVD for interconnect, diffusion, and migration 
                  barrier deposition, as well as magnetic nanomaterials design 
                  and synthesis. In 2004, he joined Lockheed Martin Space 
                  Systems Company Advanced technology Center in Palo Alto, CA 
                  developing high-temperature materials systems, nanostructured 
                  functional materials (electrical, thermal, thermoelectric), 
                  modeling quantum/superlattice structures and devices, high 
                  performance energy conversion devices (solar, high & low 
                  quality heat conversion). He holds seven patents in materials, 
                  structures and processing, two THz technology patents, with 
                  ten additional patents pending (multiple international 
                  filings) as well as four trade secrets. He has authored or 
                  co-authored over 20 archival journal publications, including 
                  book chapters in "The Chemistry of Metal CVD" as well as the 
                  "Encyclopedia of Inorganic 
            Chemistry.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2