TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Lotosky <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Lotosky <[log in to unmask]>
Date:
Fri, 20 Mar 2009 14:03:11 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
IPC 7093 - Design and Assembly Process Implementation for Leadless Surface 
Mount Components has just started - I think there was one meeting. Meeting 
notes and draft can be found on IPC Web site
Regards

Paul Lotosky
Global Director, Customer Technical Support
Cookson Electronics
109 Corporate Blvd
South Plainfield, NJ 07008
Cell 201-914-3242



Tan Geok Ang <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
03/20/2009 06:06 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Tan Geok Ang <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] LGA acceptance






Hi All, base on IPC-A-610D, there is no explicit requirement for LGA, all 
it says about Surface Mount Area Array is "for devices with solder balls 
that collapse during reflow". Is there any IPC standard/specification 
define the void on LGA? Thank you all and have a nice day!
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2