TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pete Houwen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Pete Houwen <[log in to unmask]>
Date:
Mon, 5 Apr 2010 08:49:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (18 lines)
Iain, you may have caught people on Easter Break

I am curious that you would ask about teardrops with respect to x-ray 
inspection rather than the more common use, as Gary explained.  It does make 
a little bit of sense, it could make a reference image to look at the difference 
between the copper and solder if you don't gave very high resolution x-rays.  
If that's it, I don't know if it's enough to make it worth it.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2