Good morning Les,
Rockwell Collins is one such company. Many of our military products
require a type AR coating for reworkability. We have used Humiseal 1B31
successfully on military product for many years. We have applied by HVLP
spray, automated/programmable spray, dip coating, and brush coating. You
can get the minimum 1 mil by brush coating with the as-supplied viscosity.
You have to thin the material to spray, but you can usually get the minimum
1 mil in a single pass.
Any adverse concerns (e.g., solder joints, solder mask, etc.)? Not
really. The biggest concerns are flooding of connectors as the material
spreads and wicks.
Any humidity test results? Yes. We regularly pass MIL-STD-810 and
DO-160E humidity testing.
Method of coating removal? The material dissolves in toluene so most
rework methods involve first dissolving the material in toluene.
Rework using either AR or UR coatings. We recoat with 1B31 after rework.
I have not investigated rework with a UR over 1B31.
Doug Pauls
- Bogert
<[log in to unmask]>
Sent by: TechNet To
<[log in to unmask]> [log in to unmask]
cc
03/02/2007 04:55 Subject
AM [TN] Use of Type AR Conformal
Coating for Military PCBs
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
- Bogert
<[log in to unmask]>
March 2, 2007
I am seeking info on any military folks who coat their assemblies with Type
AR coating. How do you apply it/ how many spray coats on each side of the
assembly are needed to achieve the min J-STD-001 thickness? Any adverse
concerns (e.g., solder joints, solder mask, etc.)? Any humidity test
results? method of coating removal? Rework using either AR or UR coatings.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|