TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roger Tingler <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Tingler <[log in to unmask]>
Date:
Mon, 1 May 2006 12:47:25 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (84 lines)
Eric,

The IPC-4103 equivalent for MIL-P-13949/8 (GT)
Is IPC-4103/01

Reinforcement: Woven E Glass
Resin System: PTFE
Filler: None
Permittivity Range: 2.45-2.65


Hope This Helps

Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
  540-752-5511x102
F:800-631-0856
  540-752-4832

E-mail: [log in to unmask]

"This document or these discussions contain(s) technical data under U.S.
Government export control regulations, (ITAR) 22 C.F.R. Parts 120-130, or
(EAR) 15 C.F.R. Parts 730-774. Transfer of information in this document by
any means to a foreign person or entity, whether in the U.S. or abroad,
without appropriate export authorization, is prohibited and may result in
substantial penalties."


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ekalgren
Sent: Monday, May 01, 2006 12:06 PM
To: [log in to unmask]
Subject: [TN] IPC-4103 vs. MIL-P-13949

Does anyone know if IPC-4103 has an equivalent for MIL-P-13949/8 (Type GT)
material?  If it does, I'll purchase the spec, but I'd like to know before I
throw any money away!



Thanks,



Eric Kalgren

Electrical Engineer

Continental Tool and Microwave Company

603-775-5200  ext. 333

[log in to unmask]




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2