TECHNET Archives

June 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Reuven ROKAH <[log in to unmask]>
Date:
Tue, 17 Jun 2003 07:25:58 +0300
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (66 lines)
Good design of thermal pads is a key player in such PCBs.



ROKAH Reuven




                      Werner
                      Engelmaier               To:      [log in to unmask]
                      <[log in to unmask]         cc:
                      COM>                     Subject: Re: [TN] High heat sink board hand soldering
                      Sent by: TechNet
                      <TechNet@LISTSER
                      V.IPC.ORG>


                      16/06/03 07:19
                      PM
                      Please respond
                      to "TechNet
                      E-Mail Forum.";
                      Please respond
                      to Engelmaier





Nee how Don,
1. I would preheat even higher, 110 to 115C, measured on the board.
2. I take it you talk surface pad, are your internal pads thermal-pad
designs?
3. If you have good Cu plating and no further soldering operations, and no
severe temperature cycling [in test or operation] 25 to 50% fill should be
o.k.

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2