TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 21 Sep 2009 16:47:05 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (203 lines)
Actually no, the thing about ultrasound is that at the sort of impedance
mismatch you are looking at here the realitty is that at a package to air
interface you have a virtual 100% reflection. Not sure that those
ultrasonics units are set up to use through transmission mode though,
although a couple of hours with a soldering iron and hmmmmmmmm.

Don't forget that in transmission mode all you are going to see are a number
of weaker or stronger signals delayed by the speed of ultrasound
transmission through those various materials so all you are looking for
basically is a signal.

We used a similar technique back in the '70's on the space shuttle where we
transmitted ultrasonic energy into a liquid filled bearing which was holding
a silicone rubber based wheel( imagine a skateboard wheel with the center of
the bearing filled with liquid and a probe attached to the outer sleeve of
the bearing transmitting into the liquid). We had a pair of these set up
with one set up to transmit and one to receive. The units were set up about
2 inches apart (Imagine half a roller skate with VERY soft tires) and then
ran them over the tiles of the shuttle. Once the signal disappeared you had
an air gap QED.

So in this case the transmission was from the probe, through the liquid,
into the Silicone rubber, through the tile into the skin of the shuttle
where it reflected off of the back of the outer skin in the direction of the
second probe, which when it hit it picked up the signal which was
transmitted from the skin, through the tile into the silicon rubber into the
liquid and onto the receiver.

This technique is actually very common in non destructive testing for
checking the integrity of sections of aircraft wings for delamination of the
honeycombe structure and for checking for water ingress in wing sections due
to pinholes in the outer skin.


John Burke
(408) 515 4992


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, September 21, 2009 3:17 PM
To: [log in to unmask]
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage

John and others,
But wouldn't it be even worse trying to use transmission mode because of the
nature if the circuit board underneath the component (copper barrier(s),
glass fiber bundles and epoxy?

Nobody from Sonotek or Sonoscan on TechNet?
Bev

----- Original Message -----
From: John Burke <[log in to unmask]>
To: 'TechNet E-Mail Forum' <[log in to unmask]>; Bev Christian
Sent: Mon Sep 21 18:00:16 2009
Subject: RE: [TN] Acoustic Microscopy for Under fill Coverage


 Not a discontinuity as such just an interface, and you are right, the
signal reflections will be from every interface, so for a BGA (without a
lid) the interfaces will be as follows:

1    Liquid to top of package molding compound
2    Molding compound to silicon
3    Silicon to die attach
4    Die attach to substrate
5    4 or so interfaces in the substrate itself (copper to substrate
pre-preg)
6    Substrate to under fill (or NOT!)

Depending of the acoustic impedance between the Material travelling
from/Material travelling to, more or less ultrasound energy will be
reflected at each of the interfaces.

Of the layers above I believe that the strongest reflection will be from
level 6 above.

It is 30 years since I last played with non destruct testing using
ultrasonics, but I would bet from my experiences then that you would do far
better using through transmission for this scenario rather than reflected
signals due to Bev's comment, particularly due to the substrate interface
reflections masking the ones between the package and the under fill.


John Burke
(408) 515 4992


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, September 21, 2009 2:07 PM
To: [log in to unmask]
Subject: Re: [TN] Acoustic Microscopy for Under fill Coverage

Since when can an acoustic signal punch through a BGA?  I know you can do if
for flip chips, but aren't there too many density discontinuities for CSPs
abd BGAs?
Bev

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Sep 21 14:40:48 2009
Subject: [TN] Acoustic Microscopy for Underfill Coverage

Anybody know a good lab in the North East that does acoustic microscopy? I
need to verify under fill coverage under BGAs.

Thanks,
Amol





WARNING:  Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government.  Transfer of such data by any means to
a foreign person, whether in the United States or abroad, without proper
export authorization or other approval from the U.S. Department of State is
prohibited. 
 
CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and protected
from disclosure under the law. Any unauthorized review, use, disclosure, or
distribution is prohibited. If you are not the intended recipient, please
contact the sender by reply e-mail, and delete/destroy all copies of the
original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2