TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Martin Christie <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 31 Mar 2000 16:56:00 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Rudy,

From your explanation I would assume that this process is self limiting in
terms of the amount of the deposit i.e. where you get the 0.2 micron Gold
deposit from.

Am I correct in assuming this?

Martin Christie
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
31/03/00 09:26
>James:
>
>Metals in solution are too low in electrons, and thus have a positive charge.
> Solid metals, in their shiney form, have the proper number of electrons.
>When a more "active" metal (meaning a metal that does not bind its electrons
>tightly) is immersed into a solution of a metal that does bind its electrons
>tightly, like Gold, the electrons shift from the substrate metal, (the
>substrate under Gold is almost always Nickel) to the metal in solution,
>causing the metal in solution to plate out spontaneously on to the substrate
>metal....in other words, a Nickel coated PCB, when immersed into a solution
>of Gold, will cause the Gold to plate out spontaneously on to the Nickel, and
>in the process some of the Nickel is dissolved and goes into solution.
>
>This continues until the substrate Nickel is covered, and no more Nickel is
>available for this chemical reaction, and you wind up with around 7-8
>microinches (0.2 micron) of Gold from this type of plating.
>
>Hope this helped...
>
>Rudy Sedlak
>RD Chemical Company
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2