TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Richard D. Krug" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Richard D. Krug
Date:
Wed, 24 Oct 2012 11:22:09 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
That would be fine with me.  

Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL  34602-8299
p (352) 540-4012  (Internal Ext. 2012)
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Wednesday, October 24, 2012 10:27 AM
To: [log in to unmask]
Subject: Re: [TN] White Paint Pens

Dick,

Since I would like to see what other options are out there, could we ask other users to post to the forum and sellers to post directly to you?

Steve C 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard D. Krug
Sent: Wednesday, October 24, 2012 10:16 AM
To: [log in to unmask]
Subject: [TN] White Paint Pens

The white paint pens we've been using to mark on PWB solder mask have been discontinued.  These pens required only a room temperature solvent evaporation cure.  
We've tried a couple of alternatives, but these have washed off with our wash chemistry.  I'm looking for alternatives.  

To maintain non-commercial forum, please send any specific recommendations
to me offline.   

Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL  34602-8299
p (352) 540-4012  (Internal Ext. 2012)
[log in to unmask]

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2