TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vpe2o-0000lRC; Wed, 29 Jan 97 11:43 CST
Old-Return-Path:
Date:
Wed, 29 Jan 97 09:52:37 PST
Precedence:
list
Resent-From:
From [log in to unmask] Wed Jan 29 14:
29:16 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9744
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"LhsV63.0.lJ6.1nuxo"@ipc>
Subject:
From:
"David T. Novick" <[log in to unmask]>
Cc:
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (43 lines)
We have been working with a new surface mount line for the past year and 
are happy with the different pieces of equipment.  We process many printed 
wiring assemblies some of which have 25 mil flatpacks and quadpacks 
throughout the board.  We realize that fine pitch is not as forgiving as 50 
mil pitch and through hole technology, especially when the assembly is 
fully automated.  Our challenge is that we produce a large mix of different 
assemblies, each at low volume, which we must process through the same 
surface mount line (typical batch size 10-25 boards).  This does not help 
when trying to stabilize a process.  One of our biggest issues is
coplanarity.  In most cases we do not have the luxury of receiving these
parts preformed and, therefore, must form them internally.  The handling
does not help.

We are evaluating all factors which have an effect on solder yields in an 
effort to optimize this assembly line.  We are interested in benchmarking 
with other companies in the industry.  My first question is:

What is the typical defect rate from a surface mount assembly line, when 
fine pitch components are involved, considering the narrowness of the 
process window?

And my next two questions are:

What coplanarity reqirement do you impose?

For those doing their own component lead forming, what procedures do you 
use to assure meeting this coplanarity requirement?

Rosaura Corral-Perez
[log in to unmask]    

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2