TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Darrel Therriault <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 30 Jan 2007 10:17:15 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (102 lines)
Richard/Technet,

Sorry for the confusion and my improper use of terms.

What I intended to say was we have BGAs with Pb balls.  I was wondering if 
there was an accepted process to attach those on a board that has non-Pb 
components by either reballing them with nonPb balls, using SRT rework or 
some profile that might allow both Pb and nonPb components to be run at 
the same time.

If there is no acceptable method, I either need to consume them in Pb 
assemblies (non-RoHS) or take an E&O hit on the Pb components.

DJT
 



"Stadem, Richard D." <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/30/2007 09:48 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Leaded and unleaded BGAs






By leaded/non-leaded are you speaking of LGA arrays (leadless gate
arrays) or of BGAs with SAC alloy? 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Darrel Therriault
Sent: Tuesday, January 30, 2007 10:20 AM
To: [log in to unmask]
Subject: [TN] Leaded and unleaded BGAs

Technetters,

Question for the process folks.............

We have leaded BGAs that we could use and still maintain 5/6 RoHS
compliance.

Does anyone have a process for attaching leaded and nonleaded
components?

Using SRT for the leaded parts or even reballing them with nonlead?

Is there an acceptable method for doing this or are they E & O
candidates?

Any info appreciated................DJT 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2