Richard/Technet,
Sorry for the confusion and my improper use of terms.
What I intended to say was we have BGAs with Pb balls. I was wondering if
there was an accepted process to attach those on a board that has non-Pb
components by either reballing them with nonPb balls, using SRT rework or
some profile that might allow both Pb and nonPb components to be run at
the same time.
If there is no acceptable method, I either need to consume them in Pb
assemblies (non-RoHS) or take an E&O hit on the Pb components.
DJT
"Stadem, Richard D." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/30/2007 09:48 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Leaded and unleaded BGAs
By leaded/non-leaded are you speaking of LGA arrays (leadless gate
arrays) or of BGAs with SAC alloy?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Darrel Therriault
Sent: Tuesday, January 30, 2007 10:20 AM
To: [log in to unmask]
Subject: [TN] Leaded and unleaded BGAs
Technetters,
Question for the process folks.............
We have leaded BGAs that we could use and still maintain 5/6 RoHS
compliance.
Does anyone have a process for attaching leaded and nonleaded
components?
Using SRT for the leaded parts or even reballing them with nonlead?
Is there an acceptable method for doing this or are they E & O
candidates?
Any info appreciated................DJT
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|