TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Eric Lodangco <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Sun, 5 Sep 1999 03:00:47 PHT
Content-Type:
text/plain
Parts/Attachments:
text/plain (95 lines)
Just would like to correct my item # 7 on the processes each unit will
undergo.Curing is "2 hours" minimumn not 8 hours - sorry..

Any inputs - please read my message below.

>From: Enrique Lodangco <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>,        Enrique
>Lodangco <[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Epoxy (clear or black) wicking on leads? How to control and
>            and              possible root causes.
>Date: Sun, 5 Sep 1999 01:49:53 +0800
>MIME-Version: 1.0
>From [log in to unmask] Sat Sep 04 10:49:14 1999
>Received: from [209.42.15.76] by hotmail.com (2.1) with ESMTP id
>MHotMailB99AA6970074D82197BAD12A0F4C88770; Sat Sep 04 10:49:14 1999
>Received: from jefry ([209.42.15.79])by mail.ipc.org (8.8.8+Sun/8.8.8) with
>ESMTP id MAA01480;Sat, 4 Sep 1999 12:47:51 -0500 (CDT)
>Received: from IPC.ORG by IPC.ORG (LISTSERV-TCP/IP release 1.8d) with spool
>id          2570732 for [log in to unmask]; Sat, 4 Sep 1999 12:34:20 -0500
>Received: from mail.ipc.org (209.42.15.76:34609) by IPC.ORG (LSMTP for
>Windows          NT v1.1b) with SMTP id <[log in to unmask]>; Sat, 4 Sep
>1999 12:24:20          -0500
>Received: from mail2.info.com.ph (mail2.info.com.ph [203.172.11.151]) by
>       mail.ipc.org (8.8.8+Sun/8.8.8) with ESMTP id MAA01357 for
><[log in to unmask]>; Sat, 4 Sep 1999 12:34:56 -0500 (CDT)
>Received: from ericlodangco ([203.172.28.52]) by mail2.info.com.ph
>(8.9.1a/8.9.1) with SMTP id BAA316810 for <[log in to unmask]>; Sun, 5
>  Sep 1999 01:37:55 +0800
>X-Priority: 3
>X-MSMail-Priority: Normal
>X-Mailer: Microsoft Outlook Express 5.00.2314.1300
>X-MimeOLE: Produced By Microsoft MimeOLE V5.00.2314.1300
>Message-ID:  <018c01bef6fd$e85388e0$0bc5c5c5@ericlodangco>
>Sender: TechNet <[log in to unmask]>
>
>Hi to all of you!
>
>I'm one of the new members of this forum and for a start I just would like
>to know more about controlling epoxy wicking (capillary effect) on IC
>leads.
>
>We are currently assembling module devices (Non Volatile SRAM's) for one of
>our customers. Our biggest problem now is on how to control this phenomenon
>during encapsulation process. This customer of ours have been doing this
>for almost 10 years but problem was not eliminated. They just recently
>transferred these operations (consigned everything) to us together with the
>said problem.
>
>To give you a background:
>
>1. We manufacture these SRAM's or modules using leadframes (tin plated,
>alloy 42 base metal) as the leads.
>2. Major processes these units undergo - (1) Screen printing, (2)Manual
>loading of DIPs and Lead frames onto the PCB (3) Reflow Soldering (4)
>Aqueous Cleaning (5) Manual soldering of batteries or crystal on PCB (6)
>Encapsulation - using part A and B epoxy (catalyst and resin) mixed and
>dispensed on a tub (using an encapsulation machine) where the unit will be
>inserted  (7) then cured in the oven for a minimum of 8 hours @ 70ºC.
>
>IF we are to consider that there are no handling issues and machine problem
>-
>a. how do we control this phenomenon?
>b. What are the possible root causes of this phenomenon (wicking or
>capillary effect) during encapsulation process?
>c. How do I know if it is a material problem?
>d. Effects of temperature and humidity on these Lead frames?
>
>
>Any inputs will be highly appreciated.. Thanks.
>
>For your attention:
>
>Eric Lodangco
>FASTECH ADVANCED ASSEMBLY
>Philippines
>

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2