TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 26 Apr 2000 10:48:22 +0100
Reply-To:
Michael Fenner <[log in to unmask]>
Subject:
From:
Michael Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
Organization:
Bonding Services & Products
MIME-Version:
1.0
Parts/Attachments:
text/plain (30 lines)
A eutectic alloy is
a) one which behaves like a pure or single metal on heating. In other words it melts from solid
to liquid with no transition through some pasty phase.
b) It is the lowest melting point composition.

If you have a non eutectic composition what happens on heating is the eutectic mixture will melt
and the "surplus" constituent will still be solid. A liquid with solids mixed into it is a
paste.

So if you have say, a mixture of equal portions of tin and lead (50Sn/50Pb), on heating the
eutectic (63/37) will melt into a liquid leaving the surplus lead floating around till it too
melts / dissolves.
This is what the phase diagrams you see in text books/supplier literature etc are describing.

Mike

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2