As others have said the CRX-2000 is not an inline system.
I had one at a previous job and it was a great analysis and process
development tool. Capability depends on the x-ray tube as there were
several options and the machine configuration should match the end use.
There are some automated bga inspection routines in the software, and
depending on revision, they can be somewhat useful, but not if the board has
components on the opposite side.
Apparently this is not what you are looking for.
Brad Vanderhoof
AITI
----- Original Message -----
From: <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, April 30, 2003 1:51 PM
Subject: [TN] CR Technology's CRX-2000 capability
> Fellow technetters,
>
> I'm looking for information on a X-ray system CRT CRX-2000, Does
> anybody have a brief picture of what this machine can do? and, what it's
> capabilities are? Is this a fully automated X-Ray system or only BGA
> inspection? We're basically looking for an in-line AXI with fully
automated
> inspection of BGA component, this is, a system able to inspect the
> components by using X and Y coordinates along with image/package
libraries.
>
> Your help on this matter would be really appreciated
>
> Jorge Rodriguez
> Process Engineer
> Varian Electronics Manufacturing
> 615 South River Drive
> Tempe, AZ 85281
> E-mail: [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|