TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Gerald G. Gagnon" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 14 Apr 1999 10:54:47 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Hi Technet!

Another one of those days.....

Here's my scenario:

I'm trying to design a large (18"X20"), thick (.120") complex (20+ lyr)
PWB which has two very large Land Grid Arrays (1500 pins ea.) requiring
hard nickel gold.

While the CAD routing is going on, my preference is to design the thing
using  nickel/gold as the surface finish to avoid many, many issues for
PWB mfg. We need it anyway for the LGAs.

I see boards like these (i.e. all nickel/gold finish) all over the place
when I visit board shops. Although I see some selective HASL with
nickel/gold too, NONE of the board shops want to do this and price it
accordingly.

HOWEVER, the assembly group I have to use has been using HASL for the
last 8 years but took 12 years to convert from plated reflowed tin/lead
to HASL ! I was the bozo that hung in there for the 12 years!

Nickel/gold would be a very convenient surface finish solution.

I don't have another 12 years fight left in me!

From the assemblers:

What are the SMT process differences between a HASL version (assuming it
could be built) and the nickel/gold version?


Thanks for anything that helps....

Gerry

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2