TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
"Hiteshew, Michael" <[log in to unmask]>
Date:
Thu, 29 Mar 2001 09:42:10 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, PCBA <[log in to unmask]>
Subject:
From:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (28 lines)
At 15:21 28.03.01 -0500, you wrote:
>Hi TechNetters,
>
>        I'm trying to determine how many PCB's will fit comfortably on a
>standard sheet of laminated FR4. This is for a single sided rectangular
>board 2.5" x 3.5". Here's what I need to know:
>
>1. How big is a standard sheet of FR4?

USA:  920 x 1220
Asia: 1020 x 1220 (also 1020 x 1020, 920 x 1220, 1060 x 1220)
Germany: 1060 x 1170
Italy: 1060 x 1280

These are standards. Other sizes may be available.

Jens Behrens

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2