Dear Josh:
I would recommend contacting OXFORD V.U.E, INC. at 626-256-6557. They
have lots of good data regarding etching speed, undercut, and control
methods.
Regards,
Ted Stern
[log in to unmask] wrote:
>
> I'm new at cupric etching. What are the parameters for the average innerlayer
> etch line? What controls should I be monitoring, for example, normality,
> copper content, etc? What ranges will provide me the best process in terms of
> etch line quality (minimum copper foot with best possible line width
> uniformity and etch speed)? I know equipment has a lot to do with the
> results; we can't change equipment, so I'm looking to improve quality with
> chemistry.
>
> Thanks.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|