TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Tue, 6 Nov 2012 21:44:33 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (83 lines)
So on behalf of all those hundreds if not thousands of companies that do "no
clean" and do it right, we thank you Mr. Hillman for the compliment.

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, November 06, 2012 8:27 AM
To: [log in to unmask]
Subject: Re: [TN] Limits on flux residue

Hi Wayne - no, the JSTD-001 committee has not addressed that aspect of No 
Clean processing because there are a number of product use environment 
influences and process parameters that come into play on what is 
acceptable and unacceptable. Your description would lead me to believe 
that someone has taken extreme liberty in calling something a "no clean" 
process. One of the things that we have found most interesting in the 
implementation of a no clean process for a couple of our products is that 
many folks believe "no clean" is a sloppy process and you can leave flux 
residue anywhere on the assembly in uncontrolled quantities. But the 
reality is that "no clean" solder processing requires very careful control 
of what/how much/where you allow flux residues to exist. In my view, a "no 
clean" process actually is a much tighter controlled process than a 
process that utilizes cleaning to insure that product functionality is not 
impacted.

Dave Hillman
Rockwell Collins
[log in to unmask]



From:   "Thayer, Wayne - IS" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   11/05/2012 05:52 PM
Subject:        [TN] Limits on flux residue
Sent by:        TechNet <[log in to unmask]>



Is there a spec somewhere which limits the amount of residue allowed for 
no clean processing?  I just saw a board where a BGA was about 70% 
"underfilled" by flux residue.  No, this was not a flux/underfill product! 
 A quick look at JSTD-001 Section 8 didn't seem to have specific guidance 
on this condition.

Wayne Thayer

________________________________

Email addresses of ITT Exelis employees have changed from itt.com to 
exelisinc.com. Please update your favorites and contact information to 
reflect these changes.

This e-mail and any files transmitted with it may be proprietary and are 
intended solely for the use of the individual or entity to whom they are 
addressed. If you have received this e-mail in error please notify the 
sender. Please note that any views or opinions presented in this e-mail 
are solely those of the author and do not necessarily represent those of 
Exelis Inc. The recipient should check this e-mail and any attachments for 
the presence of viruses. Exelis Inc. accepts no liability for any damage 
caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2