TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 20 Feb 2007 13:24:14 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Ramon, I assume you need a thermally conductive and adhesive-backed pad
such as SilPad for the heatsinks. There are many out there, but you need
to specify what thermal conductivity you need, the temperature rating
(what temperatures it must be able to withstand during worst-case
operation), what you intend to adhere to (metal, composite, plastic, PA,
or W) and last but far from least, the CTE factor you require. You can't
just slap anything under those parts and see if they pass functional
test. Get a Bergquist catalog or go to their website at
http://www.bergquistcompany.com/index.cfm?CFID=743285&CFTOKEN=41282313.
They have all kinds of thermally conductive "gap fillers" which can be
anything from a thermal epoxy, an adhesive backed thermally conductive
pad, electrically conductive, or electrically insulative, or a
lithium-filled grease, etc. Many of these cure at room temperature in a
few minutes. A word of caution, try to stay away from the greases and
the silicone products. 
For the stiffeners, you may wish to look at Resiweld, Eccobond, Conap,
etc. Again you need to make sure that the CTE match is appropriate, or
the stiffeners can pop off, depending on the service environment the
product is used in. These can all cure while the board is being baked to
remove moisture.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Tuesday, February 20, 2007 11:02 AM
To: [log in to unmask]
Subject: [TN] Preforms Adhesives

 

		

	Technetters:
	             Do you know of preform adhesives to bond stiffeners
or heatsinks to PWBs that do not require vacuum bags and bake, but only
bake in an oven with a proven track record?
	Regards,
	Ramon

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2