Phil
I am uncomfortable with the gold plating uniformity for 500-2000A. I'd
suggest tracking down a specialty plating house to ask their confidence on
non-pourous plated gold with 500A thickness. I recommend calling HP
(whatever their name is now) in Santa Rosa. If you find out they are
uncomfortable, you may have to sputter gold on... I have my large panel
coater company that I trust, but that's later if you need them.
Carey
-----Original Message-----
From: Phil Crepeau <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Tuesday, November 23, 1999 11:03 AM
Subject: Re: [TN] Gold plating specifications
>hi,
>
>sorry i can't answer your question, but i do have a comment. do you think
>that this thickness (thinness) of gold will provide the protection you are
>looking for?
>
>phil
>
>-----Original Message-----
>From: Scott Rebman [mailto:[log in to unmask]]
>Sent: Tuesday, November 23, 1999 8:33 AM
>To: [log in to unmask]
>Subject: [TN] Gold plating specifications
>
>
>Good day all,
>
>I am going to specify gold plating on a PCB and am curious as to how the
>rest of the world specifies such things.
>
>The board is FR-4, double sided with 2 oz copper. The quote I currently
>have is for electrolytic plating 0.05~0.20um thick. The board is
>populated with both through hole and SMT components.
>
>The purpose of going with the gold plating is to keep the pads under an
>elastomeric connector from oxidizing. Oxidation on these pads has caused
>problems with segments of an LCD becoming dim or blank.
>
>Thanks in advance for the assistance. With the exception of a few flaming
>jerks, this is a great board.
>
>Scott
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|