TECHNET Archives

January 2020

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v753.1)
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Smith <[log in to unmask]>
Date:
Mon, 27 Jan 2020 19:45:20 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII; delsp=yes; format=flowed
Parts/Attachments:
text/plain (43 lines)
with all the good answer you get.  there are good reason for Ni to be  
there.  If you use Au as solder mask - used in old days as cheap  
process, be careful about reliability - any un-dissolved gold might  
give you a headache cause preferential corrosion of exposed Cu if  
solder is not fully covered - of course, depend upon your application  
environment.  Ask your designer what is the intended usage (better  
not be pulp and paper, or gas/oil, any military application).  IMHO.  
my 1.4 cents.
jk
On Jan 27, 2020, at 5:32 PM, Steve Smith wrote:

> Hi All,
>
> I was asked today if nickel is really needed under the gold for  
> plating on copper. I have understood it that the layer of nickel  
> provides a mechanical backing for the gold layer and that it was  
> also needed for the soldering process. Is this correct and is it  
> the only reason it is used?
>
>
> My regards,
>
> Steve Smith
> Design Drafting Group Manager
> Staco Energy Products
>
> O: 937.253.1191 x158 | F: 937.253.1723
> website<http://www.stacoenergy.com/company/corporate-profile.html? 
> utm_source=signature&utm_medium=email&utm_campaign=website> |  
> map<http://www.stacoenergy.com/corporate-headquarters.html? 
> utm_source=signature&utm_medium=email&utm_campaign=map> |  
> LinkedIn<https://www.linkedin.com/company/staco-energy?trk=ppro_cprof>
>
>
> [cid:Healthcare-1908_840361ac-17f2-4e80-b79c-638c2e56eb87.png] 
> <http://www.stacoenergy.com/products-solutions/industries/ 
> healthcare.html? 
> utm_source=signature&utm_medium=email&utm_campaign=healthcare><http:// 
> www.stacoenergy.com/services/service-offerings.html? 
> utm_source=signature&utm_medium=email&utm_campaign=Promo_Service-1903>
> How are we doing? Take our survey<https://www.surveymonkey.com/r/ 
> XHK8G93>.

ATOM RSS1 RSS2