Hi Steve & Dave,
Steve, I would not warry about naming this thing, until you figure a way of
mass-producing it.
Dave, I do not under stand why this "What-cha-macallit configuration" should
fail in ATC [didn't read your paper, mea culpa]--the only CTE mismatch is in
the vertical direction, the wire, if Cu, has the same CTE as FR-4(x,y). Even in
vib, unless you hit some eigenfrequency, you should be o.k.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|