TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 7 Jul 2011 11:07:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
Parts/Attachments:
text/plain (16 lines)
We've got an assembly here showing all kinds of galvanioc corrosion after humidity tests.  Looking at the galvanic chart, I notice that gold and tin are pretty far apart.  Our tin plated shields are what's corroded.

Am I thinking too much into this?  Would ENiG on  PCB really act as the cathode for tin plating, aluminum hardware, etc.?  That would mean an awful lot of corrosion out there, there's lot's of board assemblies like this.

Pete

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2