Possible causes could be poor mixing of the mask (whipping air into the
mix), not allowing the mask to settle after mixing (not allowing air to
disappate from the mix), contaminates (in the mix, on the board) etc etc
etc...a picture of what you are seeing might help.
----- Original Message -----
From: "Stolar, Paul W" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 08, 2003 2:32 PM
Subject: [TN] Pinholes
> I am seeing pinholes in the solder mask of a board.
>
> Any words of wisdom about the cause? Or Dispensation?
>
> Paul Stolar
> Materials Engineer
> Baker Atlas
> 713-625-5376
>
> <font size="2">---------------------------------------------------<br>
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8e<br>
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet<br>
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)<br>
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest<br>
> Search the archives of previous posts at:
http://listserv.ipc.org/archives<br>
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315<br>
> -----------------------------------------------------<br></font>
>
<font size="2">---------------------------------------------------<br>
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e<br>
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet<br>
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)<br>
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest<br>
Search the archives of previous posts at: http://listserv.ipc.org/archives<br>
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315<br>
-----------------------------------------------------<br></font>
|
|
|