It seems to me too close. Is it from the centre of the pin to the edge of adjacent SMD part?
For ERSA multiflow and Inertec we use as a best robust free of wash offs 3.7- 4 mm from the edge of the selectively soldered pad to the edge of the adjacent SMD pad. For ERSA Versaflow ( single nozzle ) it can be much smaller 2.5 - 3 mm depends on configuration and layout . Other machines ( Soltec, Pillarhouse you should research ...)
Best regards
Vit Sklenar .
Robert Bosch (Australia) Pty.Ltd
RBAU-AE/MFE3
Locked Bag 66;Clayton South, VIC 3169
AUSTRALIA
Tel: +61 3 9541-7734
Fax: +61 3 9541-3909
Mob: +61 434 079 373
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Koleszar
Sent: Tuesday, 17 November 2009 4:19 AM
To: [log in to unmask]
Subject: Re: [TN] Selective Soldering Nozzle Clearance
Jack,
I use 0.100" as a target clearance. This will accommodate the majority of
machines and also selective solder pallets.
Regards,
John
John Koleszar
SMT Manager
Saline Lectronics, Inc.
710 N. Maple Rd.
Saline, MI 48170
734-944-2120 ext 294
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Monday, November 16, 2009 12:01 PM
To: [log in to unmask]
Subject: [TN] Selective Soldering Nozzle Clearance
Greetings,
For anyone who does selective soldering:
I need to design a circuit board that has a few through-hole parts that will
be soldered using a selective soldering machine, but I haven't found out
exactly which one it is yet (ELSA). Is there a DEFAULT clearance I should
keep my SMT parts away from those Through-Hole pins, or do I really have
to customize it per machine?
thanks,
Jack (aka "the new guy")
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|